Carbon Dioxide → Propylene Oxide

https://huagongshe.com/reaction/1980002

Reaction equation

Participants

RoleNameHCIDCharge
ReactantCarbon DioxideHCID 280—
ReactantWaterHCID 962—
ReactantPropyleneHCID 8252—
ProductAcetoneHCID 18039%
ProductPropylene OxideHCID 637858%
ProductPropylene CarbonateHCID 79244%

Reaction Conditions

Temperature70 °C

Reaction Steps

Thallic oxide was again prepared as in Example 1. 4.0 g of thallic oxide (8.8 mmoles), 30 g water (1.7 moles), 80 g propylene (1.9 moles) and 95 g carbon dioxide (2.2 moles) were added to the autoclave in Example 1 which was then heated to 70° C. for 2.0 hours. The analysis showed 0.81 mmoles propylene oxide (58% yield), 0.55 mmoles acetone (39% yield) and 0.06 mmoles propylene carbonate (4% yield) to have formed. 1.40 mmoles of thallous bicarbonate (16% conversion) was detected in a solution having a pH =7.9.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04483996
Source datasetuspto-grants-1984_11
ORD IDord-03ceef9447a04ba2aed307993b77fa54