Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Oxalic Acid | HCID 971 | — |
| Reactant | Oxalic acid dihydrate | HCID 61373 | — |
| Reactant | Zirconium hydroxide (Zr(OH)4), (T-4)- | HCID 84465 | — |
| Reactant | Zirconium oxide | HCID 6452892 | — |
| Solvent | Water | HCID 962 | — |
| Product | HCID 10199231 | HCID 10199231 | — |
Reaction Steps
A dispersion liquid was prepared by adding 100 g (31 g in terms of ZrO2) of zirconium hydroxide to 100 g of water, followed by well stirring. Next, as a first addition of oxalic acid, 31.7 g (a mol ratio of oxalic acid to Zr=1.0) of oxalic acid dihydrate was added to the dispersion liquid, followed by heating at 90° C. for 15 minutes. Next, as a second addition of oxalic acid, 15.8 g (a mol ratio of oxalic acid to Zr=0.5) of oxalic acid dihydrate was added to the dispersion liquid, followed by heating at 90° C. for 15 minutes to obtain a sol. When diluted to 0.5% by weight in terms of ZrO2, the zeta potential of the sol was −61 mV and the particle diameter D50 was 65 nm.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US08298979B2 |
|---|
| Source dataset | uspto-grants-2012_10 |
|---|
| ORD ID | ord-5a37bdf7b8294c1e8ce0ef4e862ec093 |
|---|
| Source note | uspto-grants-2012_10 |
|---|