HRID2068469

反应详情

EQUATION

反应方程式

HRID 2068469 的结构方程式

AUXILIARIES

试剂、催化剂与溶剂

1

CONDITIONS

反应条件

温度
90 °C

PROCEDURE

实验过程

A dispersion liquid was prepared by adding 100 g (31 g in terms of ZrO2) of zirconium hydroxide to 100 g of water, followed by well stirring. Next, as a first addition of oxalic acid, 31.7 g (a mol ratio of oxalic acid to Zr=1.0) of oxalic acid dihydrate was added to the dispersion liquid, followed by heating at 90° C. for 15 minutes. Next, as a second addition of oxalic acid, 15.8 g (a mol ratio of oxalic acid to Zr=0.5) of oxalic acid dihydrate was added to the dispersion liquid, followed by heating at 90° C. for 15 minutes to obtain a sol. When diluted to 0.5% by weight in terms of ZrO2, the zeta potential of the sol was −61 mV and the particle diameter D50 was 65 nm.

WORKUP

后处理

  1. customA dispersion liquid was prepared
  2. additionwas added to the dispersion liquid
  3. additionwas added to the dispersion liquid
  4. temperatureby heating at 90° C. for 15 minutes
  5. customto obtain a sol. When