HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 2120030Generated: October 27, 2026
Methyl Isobutyl Ketone → p-1-Ethoxyethoxystyrene p-hydroxystyrene
https://huagongshe.com/reaction/2120030
Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Methyl Isobutyl Ketone | HCID 7909 | — |
| Reactant | Ethyl vinyl ether | HCID 8023 | — |
| Reactant | 4-Ethynylphenol | HCID 32758 | — |
| Reactant | p-Toluenesulfonic acid monohydrate | HCID 521998 | — |
| Solvent | Water | HCID 962 | — |
| Product | p-1-Ethoxyethoxystyrene p-hydroxystyrene | HCID 131719558 | — |
Reaction Steps
Into a flask were charged 108.3 g of a solution of poly(p-hydroxystyrene)(weight-average molecular weight: about 15200, degree of dispersion: 1.20 (GPC method: reduced by polystyrene), 30.0 g as the weight of poly(p-hydroxystyrene)), 0.005 g of p-toluenesulfonic acid monohydrate and 102 g of methyl isobutyl ketone, and the mixture was stirred. Into this resin solution was dropped 8.7 g of ethyl vinyl ether (0.12 mol, 0.48 equivalent based on hydroxyl groups in poly(p-hydroxystyrene)) using a dropping funnel. The mixture was stirred at 25° C. for 3 hours, then, to this was added 15 g of methyl isobutylketone and 57 g of ion exchanged water, and the solution was separated. Further, the resulted organic layer was washed with 57 g of ion exchanged water and separated, four times.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06689531B2 |
|---|
| Source dataset | uspto-grants-2004_02 |
|---|
| ORD ID | ord-95972876bd2d4b5392884bee5e15eb8a |
|---|
| Source note | uspto-grants-2004_02 |
|---|