Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Phosphoric Acid | HCID 1004 | — |
| Reactant | Lauric Acid | HCID 3893 | — |
| Reactant | Glycidol | HCID 11164 | — |
| Reactant | HCID 178420821 | HCID 178420821 | — |
| Solvent | Glycerol | HCID 753 | — |
| Product | HCID 86591062 | HCID 86591062 | — |
Reaction Steps
A four-necked flask equipped with a tube for supplying nitrogen gas, a stirrer, a cooler, a thermostat, and a dropwise funnel was charged with 100.16 parts by weight of lauric acid and 0.0622 part by weight of phosphoric acid (a purity of 85%) followed by heating to 140° C. Subsequently, 222.24 parts by weight (molar ratio of glycidol/lauric acid=6) of glycidol was added drowpwise over 5 hours to allow to react until oxirane oxygen concentration in the reactant attains below 0.1% while maintaining the reaction temperature at 140° C. for 26 hours, to obtain approximately 300 parts by weight of a fatty acid esters composition of a polyglycerine (a hexaglycerine monolaurate composition). Content of the monoester was 87.7% based on the HPLC analytical condition No. 1 as described hereinabove.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06693150B1 |
|---|
| Source dataset | uspto-grants-2004_02 |
|---|
| ORD ID | ord-58734c948fde4009a80352e2e2d20cb3 |
|---|
| Source note | uspto-grants-2004_02 |
|---|