Propylene Oxide → Sodium silicate methyl methacrylate propylene oxide

https://huagongshe.com/reaction/2198476

Reaction equation

Participants

RoleNameHCIDCharge
ReactantPropylene OxideHCID 6378—
ReactantMethyl MethacrylateHCID 6658—
ReactantPhthalic AnhydrideHCID 6811—
ReactantBenzoyl PeroxideHCID 7187—
ReactantSodium HydroxideHCID 14798—
ReactantSodium orthosilicateHCID 26051—
ProductSodium silicate methyl methacrylate propylene oxideHCID 86738390—

Reaction Steps

About 50 parts by weight of an aqueous sodium silicate solution containing about 10% Na2O and 25% SiO2 by weight, 25 parts by weight of methyl methacrylate, 10 parts by weight of propylene oxide, 2 parts by weight of phthalic anhydride, 5 parts by weight of sodium hydroxide and 0.5 parts by weight of benzoyl peroxide are thoroughly mixed thereby producing an emulsion. The mixture is reacted at ambient temperature and pressure for 1 to 24 hours thereby producing a poly(sodium silicate-methyl methacrylate-propylene oxide) copolymer emulsion.