Glycine → Zinc Glycinate
Reaction equation
[NH2:1][CH2:2][C:3]([OH:5])=[O:4].[O-2].[Zn+2:7].[Zn].C(O)C(O)C>O>[NH2:1][CH2:2][C:3]([O-:5])=[O:4].[Zn+2:7].[NH2:1][CH2:2][C:3]([O-:5])=[O:4]Participants
6
Reactant 4
Product 1
Reagents, catalysts & solvents 1
Conditions
- Temperature
- 90 °C
Procedure
Thirty five (35.0) pounds of water were added to a 22 liter vessel and heated to 90° C. Glycine (4.337 lbs.) was then added with stirring, and the solution was heated to 95° C. Zinc oxide (1.766 lbs.) was then added with stirring and heating continued for two hours until the solution was clear (gly/Zn=2.7/1; PG/Zn=3.0/1). Propylene glycol (4.94 lbs.) was then added and heating continued for an additional one-half hour.
Workup
- temperaturethe solution was heated to 95° C
- stirringwith stirring
- temperatureheating
- temperatureheating
- waitcontinued for an additional one-half hour