Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 2211296Generated: October 26, 2026

Glycine → Zinc Glycinate

https://huagongshe.com/reaction/2211296

Reaction equation

Participants

RoleNameHCIDCharge
ReactantGlycineHCID 750—
ReactantPropylene GlycolHCID 1030—
ReactantZincHCID 23994—
ReactantZinc OxideHCID 3007857—
SolventWaterHCID 962—
ProductZinc GlycinateHCID 151910—

Reaction Conditions

Temperature90 °C

Reaction Steps

Thirty five (35.0) pounds of water were added to a 22 liter vessel and heated to 90° C. Glycine (4.337 lbs.) was then added with stirring, and the solution was heated to 95° C. Zinc oxide (1.766 lbs.) was then added with stirring and heating continued for two hours until the solution was clear (gly/Zn=2.7/1; PG/Zn=3.0/1). Propylene glycol (4.94 lbs.) was then added and heating continued for an additional one-half hour.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05463098
Source datasetuspto-grants-1995_10
ORD IDord-0306ac868ff940f8adf6f49d01fce92a
Source noteuspto-grants-1995_10