Styrene → HCID 18961255, compound

HRID 2255522Notes

Reaction equation

HRID 2255522 reaction equation
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[CH3:9][C:10]([C:12]([O:14][CH2:15][CH2:16][OH:17])=[O:13])=[CH2:11]>C1COCC1>[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[CH3:11][C:10]([C:12]([O:14][CH2:15][CH2:16][OH:17])=[O:13])=[CH2:9]

Participants

4

Procedure

The procedure of Example 5 was repeated. The charges of the components were as follows: CSHPU (125.0 g, 20% solids in THF), styrene (STY) (44.0 g), and HEMA (5.44 g). The solution was photolyzed for about 40 hours in order to obtain 80-85% conversion. DSC, GPC, OH equivalent weight, and other pertinent results obtained from the evaluation of the CSHPU/STY/HEMA copolymer obtained are given in Table I. The copolymer obtained was combined with CB-601 isocyanate curing agent and coated according to the procedure of Example 5. The percentage cure at room temperature was measured and set forth in Table I.

Workup

  1. customto obtain 80-85% conversion
  2. customDSC, GPC, OH equivalent weight, and other pertinent results

Sources & evidence

ORD record
ord-8fdcc80c8f154c5086899f5481236553
Source dataset
uspto-grants-1993_08
Patent number
US05240972

Reaction notes

Loading…