Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Succinic Acid | HCID 1110 | — |
| Reactant | Sodium Hydroxide | HCID 14798 | — |
| Reactant | 44742-89-4 | HCID 11593441 | — |
| Product | L-Aspartic Acid | HCID 5960 | — |
Reaction Steps
Monoammonium maleate (3.00 g of 94% wet salt, 0.0212 mole) and succinic acid (0,278 g, 0.0024 mole) were thoroughly mixed together and then were reacted as in Example 2 and 3 by heating in a convection oven at 230°240° C. for 40 minutes. A brittle, red-brown solid was obtained which weighed 2,204 g. Hydrolysis of this product with sodium hydroxide produced an aspartic acid copolymer having molecular weights by GPC of Mw 1717, Mn 1016, Mw/Mn 1.69.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US05478919 |
|---|
| Source dataset | uspto-grants-1995_12 |
|---|
| ORD ID | ord-d5adc51e1fd94b418ebb59a4e40974dc |
|---|
| Source note | uspto-grants-1995_12 |
|---|