HuagongsheHuagongshe Chemistry Print Report · For research reference only
Hydrochloric Acid → 537-03-1
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Hydrochloric Acid | HCID 313 | — |
| Reactant | Oxalic Acid | HCID 971 | — |
| Reactant | Lanthanum | HCID 23926 | — |
| Solvent | Water | HCID 962 | — |
| Product | 537-03-1 | HCID 164654 | — |
Reaction Steps
The filtrate solution containing the twice-purified lanthanum was acidified, using 200 mL of hydrochloric acid (37.5% by weight). Then a stoichiometric amount of oxalic acid in 1000 mL water was slowly added to the heated lanthanum solution (approximately 70° C.), resulting in a lanthanum oxalate precipitate. The precipitate was recovered by filtering the suspension using a sintered glass crucible of coarse porosity. The precipitate was washed with 3 liters of distilled water, dried and then heated in air to convert it to 150 g of lanthanum oxide (85% yield).
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04265862 |
| Source dataset | uspto-grants-1981_05 |
| ORD ID | ord-32a6d6e72b614ccdb3d3195d9ab1e380 |
| Source note | uspto-grants-1981_05 |