Allyl glycidyl ether → Glycidyloxypropyltrimethylsilane

https://huagongshe.com/reaction/2297070

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAllyl glycidyl etherHCID 7838—
ReactantTrimethylsilaneHCID 70435—
CatalystPlatinumHCID 23939—
ProductGlycidyloxypropyltrimethylsilaneHCID 11816314—

Reaction Conditions

Temperature130 °C

Reaction Steps

Allyl glycidyl ether (30.3 g, 0.266 moles) and 3 mg of platinum catalyst are weighed into a 300 mL laboratory autoclave. The autoclave, together with its contents, is cooled in an acetone/dry ice bath in an atmosphere of argon and 19.7 g of trimethylsilane (0.266 moles with a boiling point of 6.7° C.) are siphoned over from the condensed phase. The autoclave is closed and heated to 130° C. At the same time, the internal pressure increases to 7.6 bar and then drops again to 3.2 bar, indicating a reaction.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS06489498B2
Source datasetuspto-grants-2002_12
ORD IDord-0354b13f0ce341b786ac4f100a17fda7
Source noteuspto-grants-2002_12