Toluene → Ethylene 5norbornen-2-yl acetate

HRID 2355659Notes

Reaction equation

HRID 2355659 reaction equation
[C:1]([O:4][CH:5]1[CH2:10][CH:9]2[CH2:11][CH:6]1[CH:7]=[CH:8]2)(=[O:3])[CH3:2].C1(C)C=CC=CC=1.C=C>C1CC=CCCC=C1.C1CC=CCCC=C1.[Ni].CC(C)=O>[CH2:1]=[CH2:2].[C:1]([O:4][CH:5]1[CH2:10][CH:9]2[CH2:11][CH:6]1[CH:7]=[CH:8]2)(=[O:3])[CH3:2]

Participants

6

Conditions

Temperature
20 °C

Procedure

A glass reactor was loaded inside a glove box with L(iPr2)Ni(CH2Ph)(PMe3) (about 20 μmol; 2.00 g of 8.77 mM solution in toluene), Ni(COD)2 (about 50 μmol; 2.50 g of 17.6 mM solution in toluene), 5-norbornen-2-yl acetate (about 4.50 mmol; 3.00 g of 1.30 M solution in toluene) and toluene (about 18.45 g) such that the total volume of the toluene solution was about 30 mL. The glass reactor was sealed inside the glove box and was attached to a vacuum/nitrogen line manifold. Ethylene was fed continuously into the reactor at about 100 psi and the pressurized reaction mixture was stirred at about 20° C. Ethylene was vented after about 60 minutes and acetone was added to quench the polymerization. The precipitated polymer was collected by filtration and dried under high vacuum overnight. About 0.843 g of ethylene/5-norbornen-2-yl acetate co-polymer was obtained. The activity of the catalyst with respect to ethylene consumption was about 45 kg mol−1 h−1.

Workup

  1. customThe glass reactor was sealed inside the glove box
  2. customto quench
  3. customthe polymerization
  4. filtrationThe precipitated polymer was collected by filtration
  5. customdried under high vacuum overnight

Sources & evidence

ORD record
ord-2dc0375d14a042ccb90e7ddac769ca07
Source dataset
uspto-grants-2010_07
Patent number
US07754839B2

Reaction notes

Loading…