HRID237167

反应详情

EQUATION

反应方程式

HRID 237167 的结构方程式

AUXILIARIES

试剂、催化剂与溶剂

1

PROCEDURE

实验过程

To the aqueous polymer mixture was added 0.4 g aluminum sulfate octadecahydrate (Sigma Aldrich, Wis.) in 50 mL deionized water. The polymer mixture was then mixed for 30 minutes to provide a crosslinked polymer gel.

WORKUP

后处理

  1. additionThe polymer mixture was then mixed for 30 minutes
  2. customto provide a crosslinked polymer gel