To the aqueous polymer mixture was added 1.0 g aluminum sulfate octadecahydrate (Sigma Aldrich, Wis.) in 50 mL deionized water. The polymer mixture was then mixed for 30 minutes to provide a crosslinked polymer gel.
WORKUP
后处理
- additionThe polymer mixture was then mixed for 30 minutes
- customto provide a crosslinked polymer gel