HRID2379385

反应详情

EQUATION

反应方程式

HRID 2379385 的结构方程式

CONDITIONS

反应条件

温度
70 °C

PROCEDURE

实验过程

100 Parts of polyesterdiol which was formed from butanediol and adipic acid and had a molecular weight of about 1,000, 75 parts of diphenylmethane diisocyanate and 0.1 part of dibutyltin dilaurate were mixed, and the resultant mixture was allowed to react at 50° C. for 30 minutes and at 90° C. for 2 hours, and the reaction mixture was cooled to 70° C. Then, 26 parts of 2-hydroxyethyl methacrylate was added, and further, the resultant mixture was allowed to react for 3 hours to give urethane dimethacrylate.

WORKUP

后处理

  1. additionwere mixed
  2. customto react at 50° C. for 30 minutes and at 90° C. for 2 hours
  3. customto react for 3 hours