Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Sulfur Dioxide | HCID 1119 | — |
| Reactant | Calcium Hydroxide | HCID 6093208 | — |
| Solvent | Water | HCID 962 | — |
| Product | Calcium Sulfate | HCID 24497 | — |
| Product | Calcium sulfite | HCID 10154041 | — |
Reaction Steps
In one aspect disclosed herein there is provided a method for reducing lime consumption in DFGD systems that includes introducing lime and water into a slaker to produce a slaked lime slurry. The slaked lime slurry is subsequently introduced into a spray dryer where prior to the introduction of the slurry into the spray dryer, water is added to the slurry. Once introduced into the spray dryer, the slurry is atomized. A flue gas stream is also introduced into the spray dryer and reacts with the atomized slaked lime slurry. This reaction causes sulfur dioxide in the flue gas to be absorbed into droplets that form part of the atomized slurry. The sulfur dioxide reacts with the slaked lime in the slurry to form calcium sulfite and calcium sulfate particulate.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US08268276B2 |
|---|
| Source dataset | uspto-grants-2012_09 |
|---|
| ORD ID | ord-d44cb2ebb3b3433c85870b88f59726e2 |
|---|
| Source note | uspto-grants-2012_09 |
|---|