Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Quinone | HCID 4650 | — |
| Reactant | Toluene 2,4-Diisocyanate | HCID 11443 | — |
| Reactant | 3-Hydroxypropyl methacrylate | HCID 17694 | — |
| Solvent | Styrene | HCID 7501 | — |
| Product | Urethane acrylate | HCID 21863578 | — |
Reaction Steps
A vinyl terminated, fully reacted urethane acrylate was prepared by charging 422 parts of the oxypropylated novolac prepared in Example 1 (2.65 hydroxyl equivalents), 381 parts of hydroxypropyl methacrylate (2.65 moles), 1283 parts of styrene solvent, and 0.28 parts of p-benzoquinone inhibitor to a reactor and heating to 50° C to effect dissolution of the reactants. To the solution was added 460 parts (2.65 moles) of toluene diisocyanate (a commercially available mixture of approximately 80 percent 2,4-isomer and 20 percent 2,6-isomer) and the solution was heated and maintained at about 70° - 80° C with stirring for about 4 hours.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04107229 |
|---|
| Source dataset | uspto-grants-1978_08 |
|---|
| ORD ID | ord-d2b56232108747b38f3d5a1c8a1c8ddc |
|---|
| Source note | uspto-grants-1978_08 |
|---|