HRID247706

反应详情

EQUATION

反应方程式

HRID 247706 的结构方程式

AUXILIARIES

试剂、催化剂与溶剂

1

CONDITIONS

反应条件

温度
150 °C

PROCEDURE

实验过程

A 15:1 mole ratio of ethylene carbonate:diethylene glycol is heated with stirring under a nitrogen atmosphere for 8 hours at 150° C. using 1.0 percent Na2SnO3.3H2O as catalyst to give 95.7 percent ethylene carbonate conversion to a poly(alkylene carbonate) polyol with 21.8 percent carbon dioxide.