Reaction Steps
The epoxyoctane hydrophobic dense star polymer described in Example 10 (0.1 g) was dissolved in a mixture of 1 g of octene and 19 g of styrene. Azobisisobutyronitrile (0.15 g) was added and the resulting solution was heated at 100° C. for 0.5 day and 130° C. for 1 day to give a solid polymer.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US05393797 |
|---|
| Source dataset | uspto-grants-1995_02 |
|---|
| ORD ID | ord-80b85be3feb64a0a8bdcd101aab0a634 |
|---|
| Source note | uspto-grants-1995_02 |
|---|