- Temperature
- 130 °C
Procedure
The epoxyoctane hydrophobic dense star polymer described in Example 10 (0.1 g) was dissolved in a mixture of 1 g of octene and 19 g of styrene. Azobisisobutyronitrile (0.15 g) was added and the resulting solution was heated at 100° C. for 0.5 day and 130° C. for 1 day to give a solid polymer.
Workup
- customto give a solid polymer