HRID28075

反应详情

EQUATION

反应方程式

HRID 28075 的结构方程式

PROCEDURE

实验过程

The procedure of Part D(1) was repeated except that 0.75 gram of ethylene diacrylate was used in place of allyl acrylate. Yield: 476 grams. 2.3 weight percent of maleic anhydride was present.