HRID337397
反应详情
EQUATION
反应方程式
REACTANTS
反应物
PRODUCTS
生成物
PROCEDURE
实验过程
However, when 150 mM calcium chloride solution and 75 mM tetrasodium pyrophosphate solution, both adjusted to pH 7, were used to form the initial mixture, very small fibrous calcium pyrophosphate particles with a diameter of about 1 to 3 microns were formed. Similar results were obtained when 75 mM calcium chloride solution and 37.5 mM tetrasodium pyrophosphate solution were used to form the initial mixture.