Ethylene → HCID 20366027, compound

HRID 342797Notes

Reaction equation

HRID 342797 reaction equation
[CH2:1]=[CH:2]CCCC.[CH2:7]=[CH:8][CH2:9][CH2:10][CH2:11][CH2:12][CH2:13][CH2:14][CH2:15][CH3:16].C=C>CCCCCC>[CH2:7]=[CH:8][CH2:9][CH2:10][CH2:11][CH2:12][CH2:13][CH2:14][CH2:15][CH3:16].[CH2:1]=[CH2:2]

Participants

5

Procedure

The procedure used for the preparation of copolymer S-1 was repeated except that 1-hexene was replaced with 1-decene. A tacky amorphous polymer was obtained in 65% conversion having an inherent viscosity of 4.2 dL/g in n-hexane and a Tg of -45° C. It contained 91 mole percent of 1-decene and 9 mole percent of ethylene.

Workup

  1. customThe procedure used for the preparation of copolymer S-1
  2. customA tacky amorphous polymer was obtained in 65% conversion

Sources & evidence

ORD record
ord-8f1825e9c51041d3b604cf6789ec8c83
Source dataset
uspto-grants-1999_01
Patent number
US05859088

Reaction notes

Loading…