Phosphoric Acid → Zirconium phosphate

https://huagongshe.com/reaction/41228

Reaction equation

Participants

RoleNameHCIDCharge
ReactantPhosphoric AcidHCID 1004—
ReactantPhosphateHCID 1061—
ReactantZirconiumHCID 23995—
ProductZirconium phosphateHCID 160986—

Reaction Conditions

Temperature350 °C

Reaction Steps

A zirconium phosphate film was prepared by adding a stoichometric amount of phosphate in the form of phosphoric acid to a solution of zirconium bound to PEI. The solution was then spin coated onto a glass slide and thermally treated at 1° C. to 120° C. with a dwell time of 30 minutes followed by heating to 350° C. at 1° C./minute with a dwell time of 30 minutes followed by heating to 450° C. at 1° C./minute with a dwell time of 1 hour and then cooling to 25° C.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS08530554B1
Source datasetuspto-grants-2013_09
ORD IDord-cf4b6531eeb34d11a932e26327e1f566