HRID444190

反应详情

EQUATION

反应方程式

HRID 444190 的结构方程式

AUXILIARIES

试剂、催化剂与溶剂

1

CONDITIONS

反应条件

温度
270 °C

PROCEDURE

实验过程

2-(Hydroxymethyl)-4-methylpentanoic acid (8.7 g) is heated with 10 drops of 85% phosphonic acid in a Wood's metal bath at 220° C. for 20 minutes. A distillation head is attached and the pressure is slowly decreased to 60 mm while the temperature is increased to 270° C. Product starts to distill and the pressure is further decreased to 10 mm. The vapor temperature varies between 180° and 190° C. The yield of the title compound as distillate is 7.0 g.

WORKUP

后处理

  1. distillationto distill
  2. customThe vapor temperature varies between 180° and 190° C