L-SBR rubber is described in Publication 4242, Edition of 11/84, of Huels AG, and comprises styrene in the amount of 25 wt. %. L-SBR rubber was produced by copolymerizing 15-40 wt % styrene and correspondingly 85-60 wt. % butadiene in hexane. The Mooney viscosity ML(1+4) at 100° C. of the product was in the range 35-45. The mixture differed from the mixture of Example 2.6 only by the use of 100 parts by weight Buna® SL 705 in place of the Buna® EM 1516.