Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 465291Generated: October 30, 2026

Styrene → Styrene

https://huagongshe.com/reaction/465291

Reaction equation

Participants

RoleNameHCIDCharge
ReactantStyreneHCID 7501—
SolventHexaneHCID 8058—
ProductStyreneHCID 7501—
Product1,3-ButadieneHCID 7845—

Reaction Steps

L-SBR rubber is described in Publication 4242, Edition of 11/84, of Huels AG, and comprises styrene in the amount of 25 wt. %. L-SBR rubber was produced by copolymerizing 15-40 wt % styrene and correspondingly 85-60 wt. % butadiene in hexane. The Mooney viscosity ML(1+4) at 100° C. of the product was in the range 35-45. The mixture differed from the mixture of Example 2.6 only by the use of 100 parts by weight Buna® SL 705 in place of the Buna® EM 1516.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05153076
Source datasetuspto-grants-1992_10
ORD IDord-a3c7998455ad45edbf4d95791e4e73a9
Source noteuspto-grants-1992_10