HRID476780
反应详情
EQUATION
反应方程式
REACTANTS
反应物
PRODUCTS
生成物
AUXILIARIES
试剂、催化剂与溶剂
CONDITIONS
反应条件
- 温度
- 200 °C
PROCEDURE
实验过程
A solution containing 25 g of epoxy-cyclododecane, 1 g of lithium chloride, and 20 g of N-methyl-2-pyrrolidone was stirred at 200° C. for 6 hours. The reaction mixture contained 93.5% yield of cyclododecanone.