Used the method of Example 5, isopropenyl phosphonic acid (30.7 g, 54%, 0.14 mole), hydroxypropylacrylate (36.4 g, 0.28 mole) and water (144.9 g) were charged in the reactor. The bulk of the polymer crystallized during the first period of reflux and was found to be insoluble in water.