Styrene → Prop-2-enenitrile--ethenylbenzene (1/1)

HRID 570026Notes

Reaction equation

HRID 570026 reaction equation
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[C:9](#[N:12])[CH:10]=[CH2:11]>CN(C)C=O>[CH2:11]=[CH:10][C:9]#[N:12].[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1

Participants

4

Procedure

According to a conventional suspension polymerization procedure, styrene and acrylonitrile were polymerized to give a copolymer comprising 71% of styrene and 29% of acrylonitrile and having an intrinsic viscosity of 0.65 (30° C., dimethylformamide).

Workup

  1. customwere polymerized
  2. customto give a copolymer

Sources & evidence

ORD record
ord-e34877d34f9944d4aecc702dd0c31846
Source dataset
uspto-grants-1988_03
Patent number
US04734456

Reaction notes

Loading…