Alpha-Methylstyrene → Styrene
Reaction equation
[CH3:1][C:2](=C[CH:6]=[CH:7][C:8]1[CH:13]=[CH:12][CH:11]=[CH:10][CH:9]=1)[C:3]#[N:4].CC(C1C=CC=CC=1)=C.C(#N)C=C>>[CH2:6]=[CH:7][C:8]1[CH:13]=[CH:12][CH:11]=[CH:10][CH:9]=1.[C:3](#[N:4])[CH:2]=[CH2:1]Participants
5
Procedure
Molding was carried out using a resin composition composed of 80% by weight of α-methylstyrene-acrylonitrile copolymer having a composition consisting of 78% by weight of α-methylstyrene and 22% by weight of acrylonitrile, which contained 42% by weight of a copolymer component having a composition containing 82% by weight of α-methylstyrene, and 20% by weight of a graft copolymer obtained by graft polymerization of 60% by weight of polybutadiene rubber with 28% by weight of styrene and 12% by weight of acrylonitrile. The HDT of the resulting sample was 118° C. (Sample No. 7)