Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 637589Generated: October 27, 2026

Alpha-Methylstyrene → Styrene

https://huagongshe.com/reaction/637589

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAlpha-MethylstyreneHCID 7407—
ReactantAcrylonitrileHCID 7855—
Reactantalpha-Methyl styrene-acrylonitrileHCID 53960301—
ProductStyreneHCID 7501—
ProductAcrylonitrileHCID 7855—

Reaction Steps

Molding was carried out using a resin composition composed of 80% by weight of α-methylstyrene-acrylonitrile copolymer having a composition consisting of 78% by weight of α-methylstyrene and 22% by weight of acrylonitrile, which contained 42% by weight of a copolymer component having a composition containing 82% by weight of α-methylstyrene, and 20% by weight of a graft copolymer obtained by graft polymerization of 60% by weight of polybutadiene rubber with 28% by weight of styrene and 12% by weight of acrylonitrile. The HDT of the resulting sample was 118° C. (Sample No. 7)

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04557380
Source datasetuspto-grants-1985_12
ORD IDord-9816641413884b6883598c20d5c106ab
Source noteuspto-grants-1985_12