[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.C=CC=C.C1COCC1.[Li]CCCC>CCCCCCC>[CH2:1]=[CH:2][CH:3]=[CH2:4].[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1Participants
6
Reactant 4
Product 1
Reagents, catalysts & solvents 1
Procedure
In a first stage a butadiene-styrene copolymer is prepared by injecting 167 g of styrene, 476 g of butadiene and 2000 ppm of THF into a 10-liter reactor containing 6.4 liters of deaerated heptane. The impurities are neutralized with the aid of n-BuLi and then 0.0038 mol of n-BuLi are added, together with 0.0011 mol of sodium tert-butylate, employed as randomizing agent; the polymerization is conducted at 55° C.
Workup
- customis conducted at 55° C.