Styrene → HCID 18961255, compound
Reaction equation
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[CH3:9][C:10]([C:12]([O:14][CH2:15][CH2:16][OH:17])=[O:13])=[CH2:11]>C1COCC1>[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[CH3:11][C:10]([C:12]([O:14][CH2:15][CH2:16][OH:17])=[O:13])=[CH2:9]Participants
4
Reactant 2
Product 1
Reagents, catalysts & solvents 1
Procedure
The procedure of Example 5 was repeated. The charges of the components were as follows: CSHPU (125.0 g, 20% solids in THF), styrene (STY) (44.0 g), and HEMA (5.44 g). The solution was photolyzed for about 40 hours in order to obtain 80-85% conversion. DSC, GPC, OH equivalent weight, and other pertinent results obtained from the evaluation of the C$HPU/STY/HEMA copolymer obtained are given in Table I. The copolymer obtained was combined with CB-601 isocyanate curing agent and coated according to the procedure of Example 5. The percentage cure at room temperature was measured and set forth in Table I.
Workup
- customto obtain 80-85% conversion
- customDSC, GPC, OH equivalent weight, and other pertinent results
Sources & evidence
- ORD record
- ord-6ef52410dd1c4480a6037ccb19680715
- Source dataset
- uspto-grants-1992_06
- Patent number
- US05118580