Methyl Methacrylate → Methyl 2-methylprop-2-enoate;styrene
Reaction equation
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[C:9]([O:14][CH3:15])(=[O:13])[C:10]([CH3:12])=[CH2:11]>>[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[C:9]([O:14][CH3:15])(=[O:13])[C:10]([CH3:12])=[CH2:11]Participants
3
Procedure
According to the same procedures as described in the foregoing, a mixture of 250 parts of 0.7% aqueous solution of polyvinyl alcohol, and a solution which was obtained by dissolving 8 parts of ##STR38## into a mixed solution of 50 parts of styrene monomer and 50 parts of methyl methacrylate, was subjected to polymerization at 70° C. for 3 hours thereby obtaining 98 parts of a copolymer of styrene-methyl methacrylate.
Workup
- customa solution which was obtained
- customwas subjected to polymerization at 70° C. for 3 hours
Sources & evidence
- ORD record
- ord-6ea835cd09ab4639af7b9f587c33a8c0
- Source dataset
- uspto-grants-1981_08
- Patent number
- US04283512
Reaction notes