To 40.81 g losartan of Example 1 in 235 ml i-propanol, 3.92 g calcium hydroxide were added, and it was stirred at reflux temperature for 1 hour, and hot filtered. 410 ml n-heptane were added to the filtrate and cooled to room temperature. The solvent was decanted from a resinous residue, and 820 ml n-heptane were added. It was stirred until a white solid crystallized. It was filtered, washed with 110 ml n-heptane, and dried in vacuo at 50° C. to yield 39.2 g losartan calcium.
WORKUP
后处理
- temperatureat reflux temperature for 1 hour
- customThe solvent was decanted from a resinous residue, and 820 ml n-heptane
- additionwere added
- stirringIt was stirred until a white solid
- customcrystallized
- filtrationIt was filtered
- washwashed with 110 ml n-heptane
- customdried in vacuo at 50° C.