Itaconic acid → 2-Hydroxyethyl Methacrylate
Reaction equation
[CH2:1]([O:5]C(=O)C=C)[CH2:2]CC.[C:10]([OH:18])(=[O:17])[C:11]([CH2:13]C(O)=O)=[CH2:12].C(OS([O-])(=O)=O)CCCCCCCCCCC.[Na+]>>[CH3:13][C:11]([C:10]([O:18][CH2:2][CH2:1][OH:5])=[O:17])=[CH2:12]Participants
4
Procedure
To the solution is added 19 g butylacrylate, 3 g itaconic acid and 1 g 30% sodium laurylsulfate solution. Polymerization is carried out as described before to obtain a stable latex with essentially no coagulum.
Workup
- customPolymerization
- customto obtain a stable latex with essentially no coagulum
Sources & evidence
- ORD record
- ord-b8f700816d25410099f798738a93bd02
- Source dataset
- uspto-grants-2016_03
- Patent number
- US09290639B2
Reaction notes
Loading…