HuagongsheHuagongshe Chemistry Print Report · For research reference only
Barium bis(2-ethylhexanoate) → Barium bis(2-ethylhexanoate)
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Barium bis(2-ethylhexanoate) | HCID 102821 | — |
| Reactant | Alumina | HCID 9989226 | — |
| Solvent | Toluene | HCID 1140 | — |
| Product | Barium bis(2-ethylhexanoate) | HCID 102821 | — |
| Product | Barium | HCID 5355457 | — |
| Product | Alumina | HCID 9989226 | — |
Reaction Steps
Barium coated alpha alumina was prepared by adding 5,000 g of Alcoa A16-SG alpha alumina to a 2 liter solution of 6 wt % barium 2-ethylhexanoate in toluene. The mixture was stirred for 20 minutes. The liquid was filtered off leaving alpha alumina particles with a thin coating of barium 2-ethylhexanoate. The particles were then calcined to 500° C. for 1 hour.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US06630062B1 |
| Source dataset | uspto-grants-2003_10 |
| ORD ID | ord-9bf2715c5a4844c49bf7a5c23634deac |
| Source note | uspto-grants-2003_10 |