Molybdenum → Azane;molybdenum;tetracosahydrate

HRID 1634920
Drucken

Reaktionsgleichung

Reaktionsgleichung von HRID 1634920
[NH3:1].N.N.N.N.N.[OH2:7].O.O.O.[OH:11][Mo:12](O)(=O)=O.[OH:16][Mo](O)(=O)=O.[OH:21][Mo](O)(=O)=O.[O:26]=[Mo](=O)=O.O=[Mo](=O)=O.O=[Mo](=O)=O.O=[Mo](=O)=O.N.N.N.N.N.N.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.[Mo:72].[Mo].[Mo].[Mo].[Mo].[Mo].[Mo].[P]=O.[Mo].[P]>OP(O)(O)=O.O.[NH4+].[NH4+].[O-][Mo]([O-])(=O)=O>[NH3:1].[NH3:1].[NH3:1].[NH3:1].[NH3:1].[NH3:1].[OH2:11].[OH2:16].[OH2:21].[OH2:26].[OH2:7].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[OH2:11].[Mo:12].[Mo:12].[Mo:12].[Mo:12].[Mo:12].[Mo:12].[Mo:12].[Mo:72]=[O:7]
KomponentenVersuchsvorschriftQuellen und NachweiseNotizen zur Reaktion

Komponenten

10

Edukt 5

HCID 23932MolybdenumHCID 25488Azane;molybdenum;tetracosahydrateHCID 5462309PhosphorusHCID 6857426OxophosphanylHCID 16211167Ammonium paramolybdate tetrahydrate

Produkt 2

HCID 25488
Azane;molybdenum;tetracosahydrate
HCID 139765Molybdenum oxide

Reagenzien, Katalysatoren, Lösungsmittel 3

HCID 962WaterLösungsmittel2×HCID 1004Phosphoric AcidLösungsmittel2×HCID 61578Diammonium molybdateLösungsmittel

Versuchsvorschrift

A γ-alumina obtained as {fraction (1/16)} inch extrudates from Criterion Catalyst Company L.P., Michigan City, Ind. was used. First, an ammonium heptamolybdate solution was prepared by dissolving (NH4)6Mo7O24.4H2O in concentrated H3PO4 and water so that the ammonium molybdate concentration was 9.855 weight %, the H3PO4 concentration was 12.681 weight %, and water made up the rest. Then, 10 g of the alumina was impregnated at 25° C. with 5.32 g of the ammonium heptamolybdate solution to form a mixture. The mixture was then calcined in air at 538° C. for 6 hours to produce 10.18 g of a molybdenum oxide- and phosphorus oxide-impregnated alumina containing 2.807 weight % molybdenum and 2.096 weight % phosphorus (control catalyst).

Quellen und Nachweise

ORD-Eintrag
ord-e8f6e93665934a38aea7461a4914748e
Quelldatensatz
uspto-grants-2003_01
DOI
10.6084/m9.figshare.5104873.v1
Patentnummer
US06509289B1

Notizen zur Reaktion