Reaktionsgleichung
CC([NH:4]P([O:9][C:10]1[CH:15]=CC(Cl)=CC=1Cl)(OC)=S)C.CC([N:33]=[C:34]=[O:35])(C1C=CC=C(C([N:30]=[C:31]=[O:32])(C)C)C=1)C.[OH-].[Na+].CCN(C(C1C=CC=C(C)C=1)=O)CC>O.CC(=O)OCC>[NH2:30][C:31]([O:9][CH2:10][CH3:15])=[O:32].[NH2:4][C:34]([NH2:33])=[O:35]Komponenten
7
Edukt 4
Produkt 1
Reagenzien, Katalysatoren, Lösungsmittel 2
Versuchsvorschrift
190.8 g of Rucoflex XS-5570-55, 102.9 g of Rucoflex S-1011-55 and 6.7 g of DMPA are reacted with 48.8 g of TMXDI and 18.8 g of HDI at 80° C. for 3 hours to prepare a prepolymer. The prepolymer is then dispersed into a solution of 3.0 g of NaOH and 1.83 of EA in 650 g of water. After 10 minutes, a solution of 4.08 g of DETA in 50.0 g of water is added to form an aqueous poly(urethane/urea) dispersion. A finely divided dispersion having a solids content of 35.1% and a pH of 7.05 is obtained.
Aufarbeitung
- customto prepare a prepolymer
Quellen und Nachweise
- ORD-Eintrag
- ord-26a4abe06fa445bbb261d40a4f8d8416
- Quelldatensatz
- uspto-grants-1997_12
- Patentnummer
- US05703158
Verknüpfte Notizen
Wird geladen…