7 g of the addition compound described in Example 22, 1 g of a polysiloxane-polyalkylene glycol of Example 32 (foam stabilizer) and 200 g of a mixture of 70% by weight of crude diphenylmethane diisocyanate which had been prepared by aniline formaldehyde condensation followed by phosgenation, and 30% by weight of the distillation residue obtained from the preparation of tolylene diisocyanate were vigorously stirred together as described in Example 36. The isocyanate mixture has an isocyanate content of 29.1% and a viscosity of 1030 cP/25° C. This mixture was then heated to 150° C. for 30 minutes.