[C:1]([OH:10])(=[O:9])[CH:2]([CH:4]([C:6]([OH:8])=[O:7])[OH:5])O>O>[C@@H:4]1([C:6]([OH:8])=[O:7])[O:5][C@@H:2]1[C:1]([OH:10])=[O:9]The resulting heterogeneous reaction mixture, which was lumpy and hardened, was neutralized by addition of 15% aqueous tartaric acid solution. The polymer was filtered and a small portion was ground thoroughly. The ground material was extracted with 2-propanol for 24 hrs in a Soxhlet extractor and dried to afford a pale brown solid which was not soluble to any extent in distilled water.