Ethylene carbonate → Ethylene carbonate

HRID 247714

Reaktionsgleichung

Reaktionsgleichung von HRID 247714
[C:1]1(=[O:6])[O:5][CH2:4][CH2:3][O:2]1>O.O.O.[O-][Sn]([O-])=O.[Na+].[Na+]>[C:1]1(=[O:6])[O:5][CH2:4][CH2:3][O:2]1.[C:1](=[O:5])=[O:2]

Komponenten

4

Reaktionsbedingungen

Temperatur
175 °C

Versuchsvorschrift

A 10:1 mole ratio of ethylene carbonate to polyester poly (Formrex® 11-225, a hydroxyl functional diethylene glycol adipate, MW=500, manufactured by Witco) is heated with stirring under a nitrogen atmosphere for 3.5 hours at 175° C. using 0.5 percent sodium stannate trihydrate as catalyst to give 97.3 percent ethylene carbonate conversion to a poly(alkylene carbonate) polyol with 18.7 percent carbon dioxide. The catalyst was removed as in Example 1.

Aufarbeitung

  1. temperatureis heated

Quellen und Nachweise

ORD-Eintrag
ord-ee50f29d4fd6404fa60c2a7c438397ec
Quelldatensatz
uspto-grants-1987_11
Patentnummer
US04709069

Verknüpfte Notizen

Wird geladen…