Ethylene carbonate → Ethylene carbonate

HRID 247715

Reaktionsgleichung

Reaktionsgleichung von HRID 247715
[C:1]1(=[O:6])[O:5][CH2:4][CH2:3][O:2]1>O.O.O.[O-][Sn]([O-])=O.[Na+].[Na+]>[C:1]1(=[O:6])[O:5][CH2:4][CH2:3][O:2]1.[C:1](=[O:5])=[O:2]

Komponenten

4

Reaktionsbedingungen

Temperatur
175 °C

Versuchsvorschrift

A 10:1 mole ratio of ethylene carbonate to polyester polyol (poly(caprolactone) diol, MW=530) is heated with stirring under a nitrogen atmosphere for 4 hours at 175° C. using 0.5 percent sodium stannate trihydrate as catalyst to give 97.9 percent ethylene carbonate conversion to a poly(alkylene carbonate) polyol with 19.2 percent carbon dioxide. The catalyst is removed as in Example 1.

Quellen und Nachweise

ORD-Eintrag
ord-83e27cce764c40d789da328866ec9e7a
Quelldatensatz
uspto-grants-1987_11
Patentnummer
US04709069

Verknüpfte Notizen

Wird geladen…