Azobisisobutyronitrile → 4-(2-Methyl-2-propyl)styrene maleimide

HRID 345915
Drucken

Reaktionsgleichung

Reaktionsgleichung von HRID 345915
[C:1]1(=[O:7])[NH:5][C:4](=[O:6])[CH:3]=[CH:2]1.[CH3:8][C:9]([C:12]1[CH:19]=[CH:18][C:15]([CH:16]=[CH2:17])=[CH:14][CH:13]=1)([CH3:11])[CH3:10].N(C(C)(C)C#N)=NC(C)(C)C#N.C1(=O)CCCCC1>O>[C:4]1(=[O:6])[NH:5][C:1](=[O:7])[CH:2]=[CH:3]1.[CH3:11][C:9]([C:12]1[CH:13]=[CH:14][C:15]([CH:16]=[CH2:17])=[CH:18][CH:19]=1)([CH3:8])[CH3:10]
KomponentenReaktionsbedingungenVersuchsvorschriftAufarbeitungQuellen und NachweiseNotizen zur Reaktion

Komponenten

6

Edukt 4

HCID 6547AzobisisobutyronitrileHCID 7967CyclohexanoneHCID 10935MaleimideHCID 156274-tert-Butylstyrene

Produkt 1

HCID 867432944-(2-Methyl-2-propyl)styrene maleimideAusbeute 95 %

Reagenzien, Katalysatoren, Lösungsmittel 1

HCID 962
Water
Lösungsmittel

Reaktionsbedingungen

Temperatur
60 °C

Versuchsvorschrift

Thus, 4 g of maleimide, 6.6 g of 4-(2-methyl-2-propyl) styrene (obtained from Polysciences, Inc.), 42 mg of azobisisobutyronitrile and 40 mL of cyclohexanone were mixed and deoxygenated with argon. This solution was heated in a sealed tube at 60° C. for 4 hours. The resulting polymer was isolated by pouring the polymer solution into cold water, filtering, washing and drying under vacuum. The dried polymer (yield 95% of theoretical) had a melting point of greater than 300° C. The 1H NMR spectrum showed 0.7 NH groups for each aryl group. The polymer was soluble in aqueous alkaline solution of pH equal to 13 or higher. The relative viscosity, ηrel, was 1.15 (0.5 g of polymer per deciliter in DMF at 25° C.). As in Example 2 above, a chain transfer agent may be included to control molecular weight.

Aufarbeitung

  1. customdeoxygenated with argon
  2. customThe resulting polymer was isolated
  3. filtrationfiltering
  4. washwashing
  5. customdrying under vacuum
  6. custom1.15 (0.5 g of polymer per deciliter in DMF at 25° C.)

Quellen und Nachweise

ORD-Eintrag
ord-df3f7fa0886349a2b9ba6de8f7976a76
Quelldatensatz
uspto-grants-1991_10
DOI
10.6084/m9.figshare.5104873.v1
Patentnummer
US05059513

Notizen zur Reaktion

Auf dieser SeiteKomponentenReaktionsbedingungenVersuchsvorschriftAufarbeitungQuellen und NachweiseNotizen zur Reaktion