Reaktionsgleichung
C=C[C:3]1[CH:8]=[CH:7][C:6]([OH:9])=[C:5]([CH:10]=[CH2:11])[CH:4]=1.[CH3:12]CCCCCCCCCCCOC(CCSCCC(OCCCCCCCCCCCC)=O)=O.P(OC1C=CC=CC=1)(OC1C=CC=CC=1)OC1C=CC=CC=1.S(=O)(=O)(O)O.[OH2:74]>>[O-:74][OH:9].[C:5]1([CH:10]([CH3:11])[CH3:12])[CH:4]=[CH:3][CH:8]=[CH:7][CH:6]=1Komponenten
6
Reaktionsbedingungen
- Temperatur
- 85 °C
Versuchsvorschrift
Then, 58 g of styrenated phenol, 44 g of dilaurylthiodipropionate, and 58 g of triphenyl phosphite were added to the obtained polymer latex. The mixture was coagulated at 50° C. with an aqueous 0.25% sulfuric acid so that the latex/water ratio was 1/2, and the mixture was maintained at 85° C. for 5 minutes.
Quellen und Nachweise
- ORD-Eintrag
- ord-e1b29b3db5e546f98a7fb326188f4b59
- Quelldatensatz
- uspto-grants-1986_08
- Patentnummer
- US04604416
Verknüpfte Notizen