Reaktionsgleichung
[CH2:1]1[CH2:6]CC[CH2:3][CH2:2]1.[CH2:7]=[CH:8][C:9]1[CH:14]=[CH:13][CH:12]=[CH:11][CH:10]=1.C([Li])CCC.C=CC=C>O1CCCC1>[CH2:7]=[CH:8][C:9]1[CH:14]=[CH:13][CH:12]=[CH:11][CH:10]=1.[CH2:6]=[CH:1][CH:2]=[CH2:3].[CH2:7]=[CH:8][C:9]1[CH:14]=[CH:13][CH:12]=[CH:11][CH:10]=1Komponenten
Edukt 4
Produkt 1
Reagenzien, Katalysatoren, Lösungsmittel 1
Versuchsvorschrift
In a 2 gallon autoclave reactor, 4,500 g of cyclohexane was placed. 9 g of tetrahydrofuran, 112.5 g of styrene monomer and 1.3 g of n-butyllithium were charged into the reactor and then the reaction mixture was subjected to polymerization for 1 hour. Thereafter, 525 g of 1,3-butadiene monomer was injected into the reactor to polymerize for one hour. Finally, 112.5 g of styrene monomer was added and then polymerized for one hour to obtain styrene-butadien-styrene living block copolymer with a number average molecular weight of about 100,000 which had a styrene content of 29.9% (block styrene content of 29.5%) and 1,2-vinyl bond content of 39.6% (27.9% when reduced into whole polymer). Living lithium in the polymer was present in an amount of 1.00 mmol per 100 g of polymer.
Aufarbeitung
- customthe reaction mixture was subjected to polymerization for 1 hour
- customto polymerize for one hour
- custompolymerized for one hour
Quellen und Nachweise
- ORD-Eintrag
- ord-f7736a74c74a44e19187a776e49ec4d0
- Quelldatensatz
- uspto-grants-2000_02
- Patentnummer
- US06020439
Verknüpfte Notizen
Wird geladen…