Ethylene → Ethene propene 1-butene

HRID 503703

Reaktionsgleichung

Reaktionsgleichung von HRID 503703
C=C.[CH2:3]=[CH:4]C.[CH3:6][CH2:7][CH:8]=[CH2:9].C=C.[CH2:12]=[CH:13][CH3:14]>>[CH3:9][CH2:8][CH:7]=[CH2:6].[CH2:3]=[CH2:4].[CH2:12]=[CH:13][CH3:14]

Komponenten

5

Versuchsvorschrift

The preparation described in Example 10 was repeated with the difference that 3 g of ethylene and 5 g of propylene were fed after feeding of butene-1. During polymerization, the pressure was kept constant by feeding a 2/1 g/g ethylene/propylene mixture. The final polymer, the characterization of which is reported in Table 1, contained 1.1% wt of ethylene and 0.9% of propylene. The DSC analysis showed no melting peak.

Aufarbeitung

  1. customDuring polymerization