[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.C=CC=C.[C:13]([O:18][CH3:19])(=[O:17])[C:14]([CH3:16])=[CH2:15].C([Al](CC(C)C)OC1C(C(C)(C)C)=CC(C)=CC=1C(C)(C)C)C(C)C>>[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[C:13]([O:18][CH3:19])(=[O:17])[C:14]([CH3:16])=[CH2:15]Preparation of polystyryllithium by anionic polymerization of styrene, preparation of a polymerization initiator compound by addition reaction of butadiene, and polymerization of methyl methacrylate in the presence of an organoaluminum compound were successively performed in the same way as in Example 2 except that the temperature when diisobutyl(2,6-di-tert-butyl-4-methylphenoxy)aluminum was added, the temperature when methyl methacrylate was added, and polymerization temperature were changed from −30° C. to 0° C. and the time for polymerization of methyl methacrylate was changed from 2 hours to 1 hour.